Transcript of 008-STRUCTURAL WELDING PROCEDURE SPECIFICATION.pdf
-
Pearl GTL Project
LINDE ENGINEERING
Shell Project No: HP-3000-QAT Contractor Project No : 5887
Project Document Number: T- 4.250.999 Project Rev.: C Page 2 of 15
Purchase Order Number:
2MH127
Tag/Item Number(s): N/A
Unit(s): ASU
PCWBS: Z
-
QATAR SHELL GTL PROJECT (PEARL) C2 AIR SEPARATION UNITS CONSTRUCTION
I C 14.09.08 Ready for Construction AB EO AG RFC
H C 09.09.08 Ready for Construction AB EO AG RFC
G B 14.07.08 Issued for Company Comments AB EO AG ICC
F B 07.07.08 Issued for Company Comments AB EO AG ICC
E A 02.07.08 Issued for Company Comments AB EO AG ICC
D A 01.07.08 Issued for Company Comments AB EO AG ICC
C O 14.06.08 Issued for Company Comments AB EO AG ICC
B 11.06.08 Issued for Review BC AB AG IFR
A 10.06.08 Issued for Internal Review BC AB AG IIR
GAMA Rev.
Project Rev
Date Description Prepared
By Checked
By
Approved By
Status
No. No. ORIGINATOR
LINDE ENGINEERING AG
Document Title:
STRUCTURAL WELDING PROCEDURE SPECIFICATION
Contractor
Gama Qatar Co. W. L. L.
Document No. LOC470
GAM WPS QAC GTL 008 I
Org.
Code
Doc.
Type
Disc. Code
Geogr. Area
Seq.
No
Rev. No
Vendor Code
Project Document Number: T-4.250.999
Rev No: C
-
T-4.250.999 Rev. C Page 4 of 15
TABLE OF CONTENTS
1. 2MH127/STRWPS/013 5