This page has been reformatted by Knovel to provide easier navigation.
ALLOY INDEX
Index Terms Links
A
16-25-6
broaching 197
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
electron beam welding 173
forgeability rating 93(T)
forging temperature 93(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
solid-solution-strengthened 20
specific heat capacity 246(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength of disks as function of year of
availability 343(F)
yield strength (0.2% offset) 13(T)
17-22-A
temperature-strength capability as function of
year of availability 340(F)
Vac degassed, temperature-strength capability as
function of year of availability 340(F)
19-9DL
annealing 137(T)
composition 4(T)
density 246(T)
descaling 210
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
19-9DL (Cont.)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
strengthening mechanisms (as modified stainless
steel) 26
stress relieving 137(T)
thermal conductivity 247(T)
tensile elongation 13(T)
ultimate tensile strength 13(T)
welding and zinc removal 210
yield strength (0.2% offset) 13(T)
19-9W (AMS 5782), composition of filler metals
and electrode wires for arc welding 168(T)
A-286
aging cycles 140(T)
aircraft applications 91
annealing 137(T)
band sawing 190(T) 191(T)
broaching 196(F)
bulge forming, speed for 110(T)
carbon pickup 143
cold reduction effect on hardness 106 107(F)
cold work effect on yield strength 139(F)
composition 4(T)
composition of filler metals and electrode wires
for arc welding (AMS 5804) 168(T)
density 246(T)
draw forming, speed for 110(T)
drilling 190(T) 191(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
A-286 (Cont.)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
electric arc furnace/argon oxygen decarburization
with electroslag remelting 45(T)
electron beam welding 173
end milling 190(T) 191(T)
energy required for forging 103 104
eta phase precipitation 362(F)
eta phase role in strengthening 225
face milling 190(F,T) 191(T)
forgeability 92
forgeability rating 93(T) 102(T)
forging, aircraft turbine shaft 99(F)
forging, design guides 95(T)
forging temperature 93(T) 102(T)
forging temperature range 103
forming by spinning from a roll forging 111(F)
forming, directionality in bulging 109(F)
gamma prime precipitation for strength 26
gamma prime solvus temperature 324(T)
incipient melting temperature 324(T)
liquating phase for liquation cracking 159(T)
machinability 191 192
mean coefficient of thermal expansion 247(T)
melting range 246(T)
microstructural degradation 329
mill product availability 77
precipitation hardening 214
reaming 190(T) 191(T)
reduction rate during forging 102
restraint fixturing for heat treatment 145
rupture strength vs. Larson-Miller
parameter 248(F)
rupture strength vs. temperature 243(F)
solution treating cycles 140(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
A-286 (Cont.)
solution treating temperature 147
specific heat capacity 246(T)
straddle milling 190(T) 191(T)
stress relieving 137(T)
stress-rupture strength 14(T) 19(F)
tapping 190(T) 191(T)
tensile elongation 13(T)
tensile forming, speed for 110(T)
thermal conductivity 247(T)
threading 190(T) 191(T)
turning 190(T) 191(T) 195
ultimate tensile strength 13(T)
useable temperature, versus Al/Ti ratio in PC
castings 216(T)
vacuum induction melting with electroslag
remelting 45(T)
vacuum induction melting with vacuum arc
remelting 45(T)
weldability 153
welding 151
yield strength of disks as function of year of
availability 343(F)
yield strength (0.2% offset) 13(T)
AF 21DA
aircraft applications 119
machinability ranking 192
AF21DA-6, composition of P/M
superalloys 120(T)
AF 56 (SX 792)
composition 273(T)
density 273(T)
AF 115
aircraft applications 119
composition of P/M superalloys 120(T)
AF 1753, carbide formation 37
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
AiResist 13
composition 7(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
stress-rupture strength 19(F) 21(F)
tensile elongation 17(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
AiResist 213
composition 7(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
stress-rupture strength 19(F)
tensile elongation 13(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
AiResist 215
composition 7(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
stress-rupture strength 19(F) 21(F)
tensile elongation 17(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
AM1
composition 273(T)
density 273(T)
AM3
composition 273(T)
density 273(T)
hot isostatic pressing effect on high-cycle
fatigue (SCDS) 279(F)
AMS 5782. See also 199W.
composition of filler metals and electrode wires
for arc welding 168(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
AMS 5794. See also Multimet.
composition of filler metals and electrode wires
for arc welding 168(T)
AMS 5796. See also Haynes 25 (HS-25, L-605).
composition of filler metals and electrode wires
for arc welding 168(T)
AMS 5800. See also
composition of filler metals and electrode wires
for arc welding 168(T)
AMS 5804. See also A-286.
composition of filler metals and electrode wires
for arc welding 168(T)
AMS 5828C. See also Waspaloy.
composition of filler metals and electrode wires
for arc welding 168(T)
AP-1, fatigue crack growth rate, grain size
effect 254 256(F)
ASTM A297 grade HC
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HD
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HE
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HF
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HH
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HI
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
ASTM A297 grade HK
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HL
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HN
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HP
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HT
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HV
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HW
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A297 grade HX
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A351 grade HK-30
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A351 grade HK-40
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A351 grade HT-30
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HD50
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
ASTM A608 grade HE35
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HF30
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HH30
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HH33
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HI35
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HK30
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HK40
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HL30
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HL40
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HN40
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HT50
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HU50
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
ASTM A608 grade HW50
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ASTM A608 grade HX50
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
Astroloy. See also Udimet 700 (U-700).
aerospace applications 120(T)
aging cycles 140(T)
aging rate 156(F)
aircraft applications 91 96 97(F) 118
annealing 137(T)
cobalt addition effect 240
composition 5(T)
cyclic fatigue behavior vs. mesh size
reduction 124
density 246(T)
drilling 198 199(F) 200
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electrical resistivity 247(T)
elongation 249(T)
energy required for forging 104
extrusion 76
fatigue crack growth rate, grain size effect 254 256(F)
forgeability affected by nitrogen and oxygen
content 104
forgeability and elevated-temperature
strength 103
forgeability rating 93(T) 102(T)
forgeability vs. hardener content 103(T)
forged aircraft components 96 97(F)
forging, design guides 95(T)
forging developments 347
forging, development time requirement 104
forging temperature 93(T) 102(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Astroloy (Cont.)
grain size 249(T)
hot cracking during forging 101
hot isostatic pressed (as-HIP), aircraft
applications 119
inertia bonding 175
low-cycle fatigue strength 252
mean coefficient of thermal expansion 247(T)
melting range 246(T)
microstructural degradation 329
powder metallurgy/isothermal forging 28
powder metallurgy processing 119
reduction in area 249(T)
reduction rate during forging 102
rupture strength vs. temperature 242(F)
solution treating cycles 140(T)
specific heat capacity 246(T)
strain-controlled low-cycle fatigue properties,
wrought 253(F)
strengthening mechanisms 28
stress relieving 137(T)
stress-rupture strength 14(T)
superplastic forging 114
temperature-strength capability as function of
year of availability 340(F)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T) 249(T)
U-700 as variant of 239
yield strength (0.2% offset) 12(T) 249(T)
HIP Astroloy, strain-controlled low-cycle fatigue
properties 253(F)
LC Astroloy
aircraft applications 119
composition of P/M superalloys 120(T)
elongation 249(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
LC Astroloy (Cont.)
gamma prime solvus temperature 324(T)
grain size 249(T)
hub material for dual-alloy turbine wheel
concept 119
incipient melting temperature 324(T)
as P/M turbine disk alloys 127
prior particle boundaries corrected 119
reduction in area 249(T)
ultimate tensile strength 249(T)
vacuum (soluble gas) atomization process 122 123(F)
yield strength (0.2% offset) 249(T)
B
B-1900
aging cycles 141(T)
aircraft applications 261
aircraft applications, investment
casting 89
Al-Si coated, creep-rupture behavior 264(F)
carbide precipitation 224 362(F)
casting techniques lacking cost benefit 267
columnar grain directionally solidified, creep
behavior 270(F)
columnar grain directionally solidified,
elongation vs. temperature 279(F)
composition 6(T)
creep behavior 269 270(F)
creep elongations 263
creep-rupture strength 261 264(F)
density 262(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
ductility of cast version 263
dynamic modulus of elasticity 261(T)
forging, design guides 95(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
B-1900 (Cont.)
gamma prime solvus temperature 325(T)
hafnium addition effect 237
hot corrosion 302(F) 308
hot corrosion resistance 289
hot corrosion resistance from alloying
elements 304
hot corrosion resistance lacking 261
hot corrosion testing 292(F)
hot corrosion testing, specimen weight
change 292(F)
hot isostatic pressing 265
incipient melting temperature 325(T)
mean coefficient of thermal expansion 262(T)
mechanical properties of cast airfoils vs. cast test
bars 230 231(F)
melting range 262(T)
microstructural degradation with
overheating 328(F)
microstructure, carbides present 36(F)
microstructures after various heat treatments for
precipitation hardening 217(F)
molybdenum effect in hot corrosion 303
oxidation 297
polycrystalline, creep behavior 270(F)
polycrystalline, elongation vs.
temperature 279(F)
rupture strength vs. temperature 264(F)
solution treating cycles 141(T)
specific heat 262(T)
stress-rupture curve 259(F)
stress-rupture strength 18(T) 19(F) 20(F)
substituted for U-700 to prevent TMF
cracking 332
temperature-strength capability as function of
year of availability 340(F) 341(F) 350(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
B-1900 (Cont.)
tensile elongation 16(T)
thermal conductivity 262(T)
ultimate tensile strength 16(T)
variations developed 342
weld repair of 336
yield strength 239
yield strength (0.2% offset) 16(T)
B-1900+Hf
aging cycles 141(T)
gamma prime solvus temperature 325(T)
incipient melting temperature 325(T)
mechanical properties, cast test bars vs. cast
airfoils 230
solution treating cycles 141(T)
temperature-strength capability as function of
year of availability 341(F)
B-1910, wrought variant of B-1900, rolling 76
C
C263
aircraft applications 75(F) 76
combustor applications 75(F) 76
composition 5(T)
creep strength vs. temperature 75(F) 76
mill product availability 77
sheet product applications 75(F) 76
sheet products 91
yield strength vs. temperature 75(F) 76
Cabot 214
stress-rupture strength 14(T)
tensile elongation 12(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
CG-27, stress-rupture strength 19(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
CM-186LC
as columnar grain directionally solidified
alloy 267
cost 349
creep strength 272(F)
stress-rupture strength 260(F)
CM-247 (Ren 108) as columnar grain
directionally solidified alloy 267
CM-247LC (CGDS)
creep behavior 272
creep strength 272(F)
developed to eliminate grain-boundary
cracking 267
stress-rupture strength 260(F)
CMSX-2 (SCDS)
aging cycles 141(T)
cobalt addition effect 240
compliance constants vs. temperature 273(F)
composition 6(T) 273(T)
density 273(T)
fracture toughness for aerospace
applications 286
low-cycle fatigue behavior, thermal solidification
gradient, orientation and HIP effects 280 281(F)
as single-crystal directionally-solidified
alloy 267
solution treating cycles 141(T)
stress-rupture strength 18(T)
temperature-strength capability as function of
year of availability 350(F)
tensile elongation 17(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
CMSX-2/3 (SCDS)
creep behavior 272
stress-rupture strength 260(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
CMSX-3 (SCDS)
composition 273(T)
density 273(T)
gamma prime solvus temperature 325(T)
incipient melting temperature 325(T)
CMSX-4 (SCDS)
composition 6(T) 273(T)
creep strength 272(F)
density 273(T)
fracture toughness for aerospace
applications 286
as single-crystal directionally solidified
alloy 267
temperature range compared to CMSX-10 349
temperature-strength capability as function of
year of availability 350(F)
CMSX-6 (SCDS)
cobalt addition effect 240
composition 6(T) 273(T)
density 273(T)
as single-crystal directionally solidified
alloy 267
CMSX-10 (SCDS)
composition 6(T) 273(T)
creep strength 272(F)
density 273(T)
as single-crystal directionally solidified
alloy 267
temperature range and creep-rupture
strength 349
temperature-strength capability as function of
year of availability 350(F)
CMSX-11B (SCDS)
composition 273(T)
density 273(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
CMSX-11C (SCDS)
composition 273(T)
density 273(T)
CRM-6D, stress-rupture strength 19(F)
Custom Age 625 PLUS, composition 5(T)
D
D-6ac, face milling 190(F)
D-31 (Nb), face milling 190(F)
D-979
cold work effect on yield strength 139(F)
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
rupture strength vs. temperature 242(F)
specific heat capacity 246(T)
stress-rupture strength 14(T) 19(F)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Discaloy
aging cycles 140(T)
annealing 137(T)
composition 4(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
rupture strength vs. temperature 243(F)
solution treating cycles 140(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Discaloy (Cont.)
specific heat capacity 246(T)
stress relieving 137(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
DS 002
columnar grain directionally solidified, temperature-
strength capability as function of year of
availability, turbine blade alloys 343(F)
single-crystal directionally solidified, temperature-
strength capability as function of year of
availability, turbine blade alloys 343(F)
E
Elgiloy
density 246(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
F
FSX-414
composition 7(T)
density 262(T)
hot corrosion 308
mean coefficient of thermal expansion 262(T)
melting range 262(T)
specific heat 262(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
FSX-414 (Cont.)
stress-rupture curve 259(F)
stress-rupture strength 18(T)
tensile elongation 17(T)
thermal conductivity 262(T)
ultimate tensile strength 17(T)
yie ld strength (0.2% offset) 17(T)
G
GMR 235
composition of filler metals and electrode wires
for arc welding 168(T)
electron beam welding 173
as filler metal for IN-718 welds 167 169
friction welding 175
stress-rupture strength 18(T)
tensile elongation 17(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
Greek Ascoloy
stress-rupture strength 19(F)
temperature-strength capability as function of
year of availability 340(F)
H
Hastelloy B
composition 4(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electron beam welding 173
temperature-strength capability as function of
year of availability 350(F)
Hastelloy B-2
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Hastelloy C
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
sheet
elongation 284(T)
reduction in area 284(T)
tensile strength 284(T)
yield strength 284(T)
Hastelloy C-22
tensile elongation 12(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Hastelloy C-276
composition 4(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electric arc furnace/argon oxygen decarburization
with electroslag remelting 45(T)
Hastelloy G-30
tensile elongation 12(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Hastelloy N
composition 4(T)
electron beam welding 173
Hastelloy R-235, intergranular attack 295(F)
Hastelloy S
aging cycles 140(T)
composition 4(T)
composition of filler metals and electrode wires
for arc welding 168(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Hastelloy S (Cont.)
as filler metal (AMS 5838), base metals
involved 167
as filler metal (AMS 5838) for IN-718
welds 167
mean coefficient of thermal expansion 247(T)
melting range 246(T)
mill annealing minimum temperature 160(T)
solution annealing temperature range 160(T)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Hastelloy W
composition 4(T)
forgeability rating 93(T)
forging temperature 93(T)
Hastelloy X
aging cycles 140(T)
aircraft applications 75(F) 76
anisotropy 108(T)
annealing 137(T)
carbide precipitation 363(F)
carbides and overheating effect on mechanical
properties 326(F)
chromium content in alloy (%) 304(T)
cold reduction effect on hardness 107(F)
combustor applications 75(F) 76
composition 4(T) 6(T)
cost advantage 77
creep strength vs. temperature 75(F) 76
density 246(T)
descaling 210
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Hastelloy X (Cont.)
diffusion welding 174
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
electric arc furnace/argon oxygen decarburization
with electroslag remelting 45(T)
electron beam welding 173
Ericksen cup depth 108(T)
forgeability rating 93(T) 102(T)
forging, design guides 95(T)
forging temperature 93(T) 102(T)
forming and slotting 112
forming characteristics 108(T)
gamma prime solvus temperature 324(T)
heat treatment 146
hot corrosion 302(F)
hot corrosion resistance 304(T)
incipient melting temperature 324(T)
intergranular attack 295(F)
liquating phase for liquation cracking 159(T)
machinability 193
manufacturing ratings 194(T)
manufacturing time for part production 194(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
microstructure, carbide precipitation 329 330(F)
mill annealing minimum temperature 160(T)
mill product availability 77
Olsen cup depth 108(T)
orange peel in forming 107
oxide penetration 295(F)
precipitation hardening 213
reduction rate during forging 102
rupture strength of wrought solid-solution-
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Hastelloy X (Cont.)
strengthened nickel-base superalloys vs.
temperature 244(F)
rupture strength vs. temperature 242(F)
sheet product applications 75(F) 76
sheet products 91
solid-solution strengthened 28
solution annealing temperature range 160(T)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress relieving 137(T)
stress-rupture strength 14(T) 19(F)
temperature-strength capability as function of
year of availability 340(F)
tensile elongation 12(T)
tensile elongation vs. cold work for sheet 76(F)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
UNS number 108(T)
yield strength (0.2% offset) 12(T)
yield strength (0.2% offset) vs. cold work for
sheet 76(F)
yield strength vs. temperature 75(F) 76
Haynes alloys
density 246(T)
melting range 246(T)
specific heat capacity 246(T)
Haynes 21 (HS -21)
composition 7(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electron beam welding 173
stress-rupture strength 18(T) 19(F) 21(F)
temperature-strength capability as function of
year of availability 350(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Haynes 25 (HS -25, L-605)
aging cycles 140(T)
alloying elements effect on formability 106
annealing 137(T)
band sawing 191(T)
brazing 183 184(T)
bulge forming, speed for 110(T)
carbide precipitation 223 329
chromium content in alloy (%) 304(T)
composition 4(T) 7(T)
composition of filler metals and electrode wires
for arc welding 168(T)
density 246(T)
descaling 208
draw forming, speed for 110(T)
drilling 191(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
end milling 191(T)
explosive forming 113(F)
face milling 191(T)
as filler metal for welding 151
forgeability rating 93(T)
forging 104
forging temperature 93(T)
gamma prime solvus temperature 324(T)
G-ratio 193
hot corrosion resistance 304(T)
incipient melting temperature 324(T)
machinability 193
machinability ranking 192
manufacturing ratings 194(T)
manufacturing time for part production 194(T)
mean coefficient of thermal expansion 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Haynes 25 (HS -25, L-605) (Cont.)
melting range 246(T)
mill annealing minimum temperature 160(T)
mill product availability 77
precipitation hardening 213
reaming 191(T)
rupture strength vs. Larson-Miller
parameter 248(F)
rupture strength vs. temperature 243(F)
sheet products 91
solution annealing temperature range 160(T)
solution treating cycles 140(T)
specific heat capacity 246(T)
straddle milling 191(T)
strengthening mechanisms 29
stress relieving 137(T)
stress-rupture strength 14(T) 19(F) 21(F)
tapping 191(T)
tensile elongation 13(T)
tensile elongation vs. cold work for sheet 76(F)
tensile forming, speed for 110(T)
thermal conductivity 247(T)
threading 191(T)
turning 191(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
yield strength (0.2% offset) vs. cold work for
sheet 76(F)
Haynes 31, mill product availability 77
Haynes 95 (N-155)
annealing 137(T)
stress relieving 137(T)
Haynes 150
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Haynes 150 (Cont.)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Haynes 151 (HS -151), stress-rupture
strength 19(F) 21(F)
Haynes 188
aging cycles 140(T)
aircraft applications 75(F) 76
aircraft applications, components in F-100
engines 76(T)
alloying elements effect on formability 106
anisotropy 108(T)
cold reduction effect on hardness 106 107(F)
combustor applications 75(F) 76
composition 4(T)
composition of filler metals and electrode wires
for arc welding 168(T)
creep-buckling resistance 76(T)
creep life 76(T)
creep strength vs. temperature 75(F) 76
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
Ericksen cup depth 108(T)
forgeability rating 93(T)
forging temperature 93(T)
forming characteristics 108(T)
gamma prime solvus temperature 324(T)
higher-temperature alternative to Hastelloy X 77
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Haynes 188 (Cont.)
high-temperature strength 76(T)
hot corrosion 302(F)
incipient melting temperature 324(T)
lanthanum inclusions, effect on oxidation 297
low-cycle fatigue strength 76(T)
mean coefficient of thermal expansion 247(T)
microstructure, carbide precipitation after
overheating 327(F)
mill annealing minimum temperature 160(T)
mill product availability 77
Olsen cup depth 108(T)
oxidation resistance 76(T)
oxidation resistance improved by aluminide
coating 314
rupture strength vs. Larson-Miller
parameter 248(F)
rupture strength vs. temperature 243(F)
sheet product applications 75(F) 76
sheet products 91
solution annealing temperature range 160(T)
solution treating cycles 140(T)
stress-rupture strength 14(T)
temperature-strength capability as function of
year of availability 340(F)
tensile elongation 13(T)
tensile elongation vs. cold work for sheet 76(F)
thermal conductivity 247(T)
thermal fatigue 76(T)
ultimate tensile strength 13(T)
UNS number 108(T)
welding 151
yield strength (0.2% offset) 13(T)
yield strength (0.2% offset) vs. cold work for
sheet 76(F)
yield strength vs. temperature 75(F) 76
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Haynes 214
alloying elements effects on formability 106
cold reduction effect on hardness 107(F)
composition 4(T)
mill product availability 77
Haynes 230
alloying elements effects on formability 106
anisotropy 108(T)
cold reduction effect on hardness 107(F)
composition 4(T)
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
Ericksen cup depth 108(T)
forming characteristics 108(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
mill annealing minimum temperature 160(T)
Olsen cup depth 108(T)
solution annealing temperature range 160(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 12(T)
tensile elongation vs. cold work for sheet 76(F)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
UNS number 108(T)
yield strength (0.2% offset) 12(T)
yield strength (0.2% offset) vs. cold work for
sheet 76(F)
Haynes 242, composition 5(T)
Haynes 263, composition 5(T)
Haynes 556
aging cycles 140(T)
composition 4(T)
composition of filler metals and electrode wires
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Haynes 556 (Cont.)
for arc welding 168(T)
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Haynes 1002
density 262(T)
dynamic modulus of elasticity 261(T)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
specific heat 262(T)
tensile elongation 17(T)
thermal conductivity 262(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
Haynes HR-120, composition 4(T)
Haynes HR-160, composition 4(T)
Haynes R-41, composition 5(T)
Haynes Stellite 31 (HS -31, X-40). See also
X-40 1
electron beam welding 173
grinding fluid effect on grinding ratio 202(T)
HIP Astroloy. See entry after Astroloy.
I
IN-120, magnesium addition effect on stress-
rupture behavior 238(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
IN-162
density 262(T)
dynamic modulus of elasticity 261(T)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
specific heat 262(T)
stress-rupture strength 18(T)
tensile elongation 16(T)
thermal conductivity 262(T)
ultimate tensile strength 16(T)
yield strength (0.2% offset) 16(T)
IN 591, temperature-strength capability as function
of year of availability 350(F)
IN-731
density 262(T)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
specific heat 262(T)
stress-rupture strength 18(T)
tensile elongation 16(T)
thermal conductivity 262(T)
ultimate tensile strength 16(T)
yield strength (0.2% offset) 16(T)
IN 935, temperature-strength capability as function
of year of availability 350(F)
IN-939
aging cycles 141(T)
aircraft applications 227 261
cast in case-type components 348
hot corrosion 308
hot corrosion resistance 307
for industrial and marine turbines 263
oxidation, amorphous silica effect 351(F)
oxidation-resistance potential 351
solution treating cycles 141(T)
stress-rupture strength 18(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
IN-939 (Cont.)
temperature-strength capability as function of
year of availability 350(F)
tensile elongation 17(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
IN 6201, temperature-strength capability as
function of year of availability 350(F)
IN 6202, temperature-strength capability as
function of year of availability 350(F)
IN 6203, temperature-strength capability as
function of year of availability 350(F)
Inco alloy 330
creep-rupture strength 241
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
INCO 728
hot corrosion testing 292(F)
hot corrosion testing, specimen weight
change 292(F)
Incoloy 800
annealing 137(T)
cold reduction effect on hardness 107(F)
composition 4(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
specific heat capacity 246(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Incoloy 800 (Cont.)
stress relieving 137(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 800H
annealing 137(T)
composition 4(T)
strengthening mechanis ms 26
stress relieving 137(T)
Incoloy 800HT
composition 4(T)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
Incoloy 801
composition 4(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 802
composition 4(T)
density 246(T)
drilling hole sizes 199(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Incoloy 802 (Cont.)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 807
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 825
annealing 137(T)
density 246(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
stress relieving 137(T)
tensile elongation 13(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Incoloy 825 (Cont.)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 901
annealing 137(T)
composition 5(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
fine grain, temperature-strength capability as
function of year of availability 340(F)
forgeability rating 93(T)
forging, grain-size variations 104
forging temperature 93(T)
gamma prime precipitation for strength 26
high-cycle fatigue, grain size effect 257(T)
high-cycle fatigue, surface
condition effect 257(T)
low-cycle fatigue, grain size effect 251 252(T)
machinability ranking 192
microstructural degradation 329
precipitation hardening 214
stress relieving 137(T)
stress-rupture strength 19(F)
temperature-strength capability as function of
year of availability 340(F)
Incoloy 903
composition 4(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Incoloy 903 (Cont.)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 904
density 246(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
thermal conductivity 247(T)
Incoloy 907
composition 4(T)
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 909
composition 4(T)
density 246(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
strengthening mechanisms 28
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Incoloy 909 (Cont.)
ultimate tensile strength 13(T)
yield strength (0.2% offset) 13(T)
Incoloy 925
composition 4(T)
electric arc furnace/argon oxygen decarburization
with electroslag remelting 45(T)
Incoloy MA-956
brazing 183
as common ODS alloy 129
composition 129(T) 132
creep-rupture strength 243(F) 244(F)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electrical resistivity 250(T)
elongation (%) 250(T)
grain structure 132
heat treatment industry applications 133
mean coefficient of thermal expansion at
538 C 250(T)
melting range 250(T)
1000h rupture strength 250(T)
product forms available 132(T)
reduction in area at 1095C 250(T)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
rupture strength vs. temperature 243(F)
sheet form available 132
specific heat capacity at 21 C 250(T)
thermal conductivity at 21 C 250(T)
ultimate tensile strength 250(T)
yield strength 250(T)
Inconel alloys
descaling 208(T)
development 1 339
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel alloys (Cont.)
nitrogen pickup 143(F)
sheet products 91
solid-solution-strengthened 20
Inconel 82, as filler metal for IN-718 welds 167
Inconel 100 (IN -100)
aerospace applications 120(T)
aging cycles 141(T)
aircraft applications 261
aircraft applications, investment casting 89
applications, high-temperature 23
availability 342
casting techniques lacking cost benefit 267
centrifugal atomization for P/M processing 122
chromium content in alloy (%) 304(T)
chromium content low for turbine disk
applications 344
cobalt addition effect 240
columnar grain directionally solidified, creep
behavior 270(F)
columnar grain directionally solidified,
elongation vs. temperature 279(F)
composition 5(T) 6(T)
composition of P/M superalloys 120(T)
creep behavior 269 270(F)
data compilation 261 263
density 262(T)
drilling 200
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 261(T)
elongation 249(T)
forging, development time requirement 104
forging temperatures 102
gamma-gamma prime eutectic, white islands
of 360(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 100 (IN -100) (Cont.)
gamma prime solvus temperature. 324(T) 325(T)
gatorized, rupture strength vs.
temperature 242(F) 264(F)
grain size 249(T)
G-ratio 193
hot corrosion 302(F) 308
hot corrosion resistance 289 304(T)
hot corrosion resistance from alloying
elements 304
hot corrosion testing 292(F)
hot corrosion testing, specimen weight
change 292(F)
incipient melting temperature 324(T) 325(T)
machinability 192
mean coefficient of thermal expansion 262(T)
mechanical properties, cast test bars vs. cast
airfoils 230
melting range 262(T)
microstructural degradation 329
Mod, temperature-strength capability as function
of year of availability 340(F)
physical property data not available 241
polycrystalline, creep behavior 270(F)
polycrystalline, elongation vs.
temperature 279(F)
polycrystalline, temperature-strength capability as
function of year of availability, turbine blade
alloys 343(F)
powder metallurgy form, yo-yo heat
treatment 217
powder metallurgy/isothermal forging 28
powder metallurgy processing 117 119 342
powder metallurgy processing and forging 102
as powder metallurgy turbine disk alloys 127
powder processing with superplastic
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 100 (IN -100) (Cont.)
forming 115
precipitation hardening 214
reduction in area 249(T)
rupture strength vs. temperature 264(F)
sigma phase formation 362(F)
solution treating cycles 141(T)
specific heat 262(T)
strain-controlled low-cycle fatigue
properties 253(F)
stress-rupture curve 259(F)
stress-rupture strength 18(T) 19(F) 20(F) 272(F)
temperature-strength capability as function of
year of availability 340(F) 341(F) 350(F)
tensile elongation 16(T)
tensile strength, and conversion from cast to
wrought form 243
tensile strength, cast vs. wrought forms 227
tensile yield strength 278(F)
thermal conductivity 262(T)
ultimate tensile strength 16(T) 249(T)
vacuum (soluble gas) atomization
process 122 123(F)
vanadium effect in hot corrosion 303
yield strength 239
yield strength (0.2% offset) 16(T) 249(T)
Inconel 102
composition 5(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
magnesium addition effect on creep rupture
life 238
Inconel 117, composition of filler metals and
electrode wires for arc welding 168(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 587
dynamic modulus of elasticity 245(T)
stress-rupture strength 14(T)
tensile elongation 12(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Inconel 596, dynamic modulus of
elasticity 245(T)
Inconel 597
density 246(T)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Inconel 600
aging cycles 140(T)
annealing 137(T)
bar, elongation 284(T)
bar, reduction in area 284(T)
bar, tensile strength 284(T)
bar, yield strength 284(T)
brazing 182
cold reduction effect on hardness 107(F)
composition 4(T)
density 246(T)
descaling 210
diffusion welding 174
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 600 (Cont.)
electric arc furnace/argon oxygen
decarburization with electroslag
remelting 45(T)
electron beam welding 173
filler metals used for welds 167
forgeability 104
forgeability rating 93(T)
forging temperature 93(T)
liquating phase for liquation cracking 159(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
rupture strength vs. temperature 242(F)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress relieving 137(T)
stress-rupture strength 14(T)
temperature-strength capability as function of
year of availability 340(F)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Inconel 601
aging cycles 140(T)
annealing 137(T)
composition 4(T)
composition of filler metals and electrode wires
for arc welding 168(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 601 (Cont.)
electrical resistivity 247(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
rupture strength vs. temperature 242(F)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress relieving 137(T)
stress-rupture strength 14(T)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Inconel 617
aging cycles 140(T)
aircraft applications 75(F) 76
combustor applications 75(F) 76
composition 4(T)
composition of filler metals and electrode
wires for arc welding 168(T)
creep strength vs. temperature 75(F) 76
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
gamma prime solvus temperature 324(T)
incipient melting temperature 324(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
microstructure, incipient melting effect 326(F)
mill annealing minimum temperature 160(T)
mill product availability 77
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 617 (Cont.)
rupture strength of wrought solid-solution-
strengthened nickel-base superalloys vs.
temperature 244(F)
sheet product applications 75(F) 76
solution annealing temperature range 160(T)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 12(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
yield strength vs. temperature 75(F) 76
Inconel 625
aging cycles 140(T)
anisotropy 108(T)
annealing 137(T)
cast, density 262(T)
cast, mean coefficient of thermal
expansion 262(T)
cast, melting range 262(T)
cast, specific heat 262(T)
cast, thermal conductivity 262(T)
composition 4(T)
density 246(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
electric arc furnace/argon oxygen decarburization
with electroslag remelting 45(T)
electron beam welding 173
Ericksen cup depth 108(T)
forming characteristics 108(T)
gamma prime solvus temperature 324(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 625 (Cont.)
incipient melting temperature 324(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
mill annealing minimum temperature 160(T)
mill product availability 77
Olsen cup depth 108(T)
rupture strength vs. temperature 242(F)
solid-solution-strengthened 28
solution annealing temperature range 160(T)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress relieving 137(T)
stress-rupture strength 14(T) 18(T)
tensile elongation 12(T) 16(T)
tensile elongation vs. cold work for sheet 76(F)
thermal conductivity 247(T)
ultimate tensile strength 12(T) 16(T)
UNS number 108(T)
vacuum induction melting with electroslag
remelting 45(T)
vacuum induction melting with vacuum arc
remelting 45(T)
yield strength (0.2% offset) 12(T) 16(T)
yield strength (0.2% offset) vs. cold work for
sheet 76(F)
Inconel 690
annealing 137(T)
density 246(T)
electrical resistivity 247(T)
mean coefficent of thermal expansion 247(T)
melting range 246(T)
specific heat capacity 246(T)
stress relieving 137(T)
thermal conductivity 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 700
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electron beam welding (not U-700) 173
face milling 190(F)
forgeability rating 93(T)
forging temperature93(T)
Inconel 702
composition 5(T)
weldability as function of aluminum and
titanium hardener content 155(F)
Inconel 706 (IN -706)
aging cycles 140(T)
composition 5(T)
composition of P/M superalloys 120(T)
density 246(T)
development 343
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
eta phase disposed, fatigue life affected 253(F)
forged billets, elongation 284(T)
forged billets, reduction in area 284(T)
forged billets, tensile strength 284(T)
forged billets, yield strength 284(T)
forging, fracture toughness 285(T)
forging, roo m-temperature yield strength 285(T)
forging-weldment, fracture toughness 285(T)
forging-weldment, room-temperature yield
strength 285(T)
gamma double-prime phase effect on
strengthening 226
gamma double-prime precipitate 34
mean coefficient of thermal expansion 247(T)
melting range 246(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 706 (IN -706) (Cont.)
niobium as gamma prime strengthener 154
no PWHT cracking 155
postweld heat treat cracking of welds 154
solution treating cycles 140(T)
specific heat capacity 246(T)
strengthening mechanisms 28
stress-rupture strength 14(T)
tensile elongation 12(T)
tensile properties 12(T) 283 284(T) 285(T)
thermal conductivity 247(T)
ultimate tensile strength 12(T)
vacuum induction melting with electroslag
remelting 45(T)
vacuum induction melting with electroslag
remelting and vacuum arc remelting 45(T)
vacuum induction melting with vacuum arc
remelting 45(T)
yield strength (0.2% offset) 12(T)
Inconel 713 (IN -713)
aging cycles 141(T)
aircraft applications 261
applications, high-temperature 23
chromium content in alloy (%) 304(T)
cobalt addition effect 240
development 339 341
friction welding 175
hot corrosion 304 305(F)
hot corrosion resistance 304(T)
hot corrosion resistance, aluminide-type coating
applied 311
investment casting, polycrystalline 89
nickel-aluminide-type coating effect on hot
corrosion resistance 304 305(F)
solution treating cycles 141(T)
strengthening mechanisms 28
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 713 (IN -713) (Cont.)
temperature-strength capability as function of
year of availability 340(F) 341(F)
IN-713C
composition 6(T)
density 262(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 261(T)
electron beam welding 173
friction welding 175
gamma prime solvus temperature 325(T)
incipient melting temperature 325(T)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
oxidation 297
rupture strength vs. temperature 264(F)
specific heat 262(T)
stress-rupture curve 259(F)
stress-rupture strength 18(T) 19(F)
tcp phases formed 357
temperature-strength capability as function of
year of availability 350(F)
temperature-strength capability as function of
year of availability, turbine blade
alloys 343(F)
tensile elongation 16(T)
thermal conductivity 262(T)
ultimate tensile strength 16(T)
yield strength (0.2% offset) 16(T)
IN-713 Hf
stress-rupture strength 18(T)
tensile elongation 17(T)
ultimate tensile strength 17(T)
yield strength (0.2% offset) 17(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 713LC (IN-713LC)
aircraft applications 261
composition 6(T)
density 262(T)
dynamic modulus of elasticity 261(T)
gamma prime solvus temperature 325(T)
incipient melting temperature 325(T)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
specific heat 262(T)
stress-rupture strength 18(T)
tensile elongation 16(T)
thermal conductivity 262(T)
ultimate tensile strength 16(T)
yield strength (0.2% offset) 16(T)
Inconel 718 (IN -718)
aerospace applications 248
aging cycles 140(T) 141(T)
aging rate 156(F)
aircraft applications 24 152 227
annealing 137(T)
availability 24
bar, elongation 284(T)
bar, fracture toughness 285(T)
bar, reduction in area 284(T)
bar, room-temperature yield strength 285(T)
bar, tensile strength 284(T)
bar, yield strength 284(T)
brazing 183
carbide precipitation 361(F)
cobalt addition effect 240
cogging 75
composition 5(T) 6(T)
composition of filler metals and electrode wires
for arc welding 168(T)
composition of P/M superalloys 120(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 718 (IN -718) (Cont.)
cost 8 24
cost of materials for destructive test
methods 346
delta, gamma and gamma double-prime
phases 361(F)
delta phase role in preventing stress-rupture
embrittlement 225 (F)
delta phase role in strengthening 225 (F) 227(T)
delta solvus 75
density 246(T)
diffusion welding 174
discrete white spots 64 65(F)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
electron beam welding 173
elongation 249(T)
explosive forming 112(F)
fatigue crack growth rate 253 (F)
fatigue crack growth rate, environment
effects 255 257(F)
as filler metal for IN-718 welds 167
fine grain forged 103
forgeability 24
forgeability rating 93(T) 102(T)
forging 97 98(F)
forging, bands caused by too high
temperature 99 102(F)
forging, design guides 95(T)
forging, elongation 284(T)
forging, fracture toughness 285(T)
forging, GTA weld in, elongation 284(T)
forging, GTA weld in, reduction in area 284(T)
forging, GTA weld in, tensile strength 284(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 718 (IN -718) (Cont.)
forging, GTA weld in, yield strength 284(T)
forging prior to peeling the billet surface 64(F)
forging, room-temperature yield strength 285(T)
forgings, reduction in area 284(T)
forgings, tensile strength 284(T)
forging temperature 93(T) 99 101(F) 102(T)
forging to three distinctly different
structures 103
forging-weldment, fracture toughness 285(T)
forging-weldment, room-temperature yield
strength 285(T)
forging, yield strength 284(T)
freckle structure 41(F)
friction welding 175
gamma double-prime phase 27
gamma double-prime precipitate 34 218
gamma prime precipitation for strength 26
grain size 249(T)
grain size prediction by mo deling 347
G-ratio 193
hardening retarded 155(F)
heat treatment 136 245 248 251(F)
high strength (HS), tensile and stress-rupture
properties 249 251(F)
homogenization of cast product 73(F)
ingot-metallurgy 348
investment casting 80
for large structural castings 348
lead content effect on tensile properties 234 236(F) 237(T)
liquation cracking 157 158(F)
low-cycle fatigue strength 251
machinability ranking 192
magnesium addition effect on stress-rupture
ductility 238
mean coefficient of thermal expansion 247(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 718 (IN -718) (Cont.)
melting range 246(T)
microstructural degradation 329
microstructure 33(F)
mill product availability 77
mushy-zone thickness vs. ingot diameter 43(F)
niobium as gamma prime strengthener 154
niobium content 41(F) 43
no PWHT cracking 155
notch ductility lacked 218
notch sensitivity 226 227(T)
overaged, crystal structure and 27(T)
postweld heat treat cracking of welds 154
precipitation hardening 212
process modeling of remelt ingots 345
production size capability 343
pseudobinary phase diagram 41 42(F) 43
reduction in area 249(T)
reduction rate during forging 102
rupture strength vs. temperature 242(F)
sheet, elongation 284(T)
sheet, GTA weld in, elongation 284(T)
sheet, GTA weld in, reduction in area 284(T)
sheet, GTA weld in, tensile strength 284(T)
sheet, GTA weld in, yield strength 284(T)
sheet, reduction in area 284(T)
sheet, tensile strength 284(T)
sheet, yield strength 284(T)
solidification white spots 65(F) 67(F)
solution treating cycles 140(T) 141(T)
solution treating temperature 147
specific heat capacity 246(T)
standard forged 103
standard heat treatment (STD) 248
standard heat treatment, tensile and stress-rupture
properties 249 251(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 718 (IN -718) (Cont.)
strain-age (PWHT) cracking prevention 155
strengthening mechanisms 28
stress relieving 137(T)
stress-rupture strength 14(T) 19(F)
superplastic forming 113(F)
tensile elongation 12(T) 16(T)
tensile properties 244 249(T) 283 284(T)
285(T)
thermal conductivity 247(T)
time -temperature-transformation diagram 105(F)
tramp element concentrations allowable 235 237(T)
triple-melted ingot processing 72
ultimate tensile strength 12(T) 16(T) 249(T)
vacuum arc remelting 63(F)
vacuum induction melting with electroslag remelting 45(T)
vacuum induction melting with electroslag
remelting and vacuum arc remelting 45(T)
vacuum induction melting with vacuum arc
remelting 45(T)
weldability as function of aluminum and
titanium hardener content 155(F)
welding 149 151 186(F) 187
welding, filler metal choices 167 169
wrought form 2
yield strength of disks as function of year of
availability 343(F)
yield strength (0.2% offset) 12(T)
Inconel 718 Direct Age
forged 103
forged structure 105
stress-rupture strength 14(T)
tensile and stress-rupture properties 249 251(F)
tensile elongation 12(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
IN-718 SPF
grain growth vs. time 113 114(F)
superplastic-formed product 113(F)
Inconel 718 Super
stress-rupture strength 14(T)
tensile elongation 12(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Inconel 721, composition 5(T)
Inconel 722, composition 5(T)
Inconel 725, composition 5(T)
Inconel 738 (IN -738)
aging cycles 141(T)
aircraft applications 261
composition 6(T)
density 262(T)
directionally solidified 343
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 261(T)
hot corrosion 302(F) 308
hot corrosion resistance 304 307
hot isostatic pressing, and stress-rupture
strength 265(F)
low-cycle fatigue behavior, atmosphere
effects 255 257(F)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
rupture strength vs. temperature 264(F)
solution treating cycles 141(T)
specific heat 262(T)
stress-rupture curve 259(F)
stress-rupture strength 19(F) 20(F)
temperature-strength capability as function of
year of availability 350(F)
tensile elongation 16(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 738 (IN -738) (Cont.)
thermal conductivity 262(T)
ultimate tensile strength 16(T)
yield strength (0.2% offset) 16(T)
IN-738C, stress-rupture strength 18(T)
IN-738LC
gamma prime solvus temperature 325(T)
hot isostatic pressing effect on creep
behavior 335(F)
incipient melting temperature 325(T)
stress-rupture strength 18(T)
weld repair of 336
Inconel X-750
aging cycles (AMS 5667) 140(T)
aging cycles (AMS 5668) 140(T)
annealing 137(T)
band sawing 191(T)
bar, elongation 284(T)
bar, reduction in area 284(T)
bar, tensile strength 284(T)
bar, yield strength 284(T)
cold reduction effect on hardness 107(F)
cold work effect on yield strength 139(F)
composition 5(T)
density 246(T)
descaling 210
drilling 191(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
electron beam welding 173
end milling 191(T)
face milling 191(T)
forgeability rating 93(T)
forged billet, GTA weld in, elongation 284(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel X-750 (Cont.)
forged billet, GTA weld in, reduction in
area 284(T)
forged billet, GTA weld in, tensile
strength 284(T)
forged billet, GTA weld in, yield
strength 284(T)
forging, fracture toughness 285(T)
forging, room-temperature yield strength 285(T)
forging temperature 93(T)
forging-weldment, fracture toughness 285(T)
forging-weldment, room-temperature yield
strength 285(T)
gamma prime solvus temperature 324(T)
incipient melting temperature 324(T)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
metallic contaminants for 203
mill product availability 77
reaming 191(T)
rupture strength vs. temperature 242(F)
sheet, elongation 284(T)
sheet, GTA weld in, elongation 284(T)
sheet, GTA weld in, reduction in area 284(T)
sheet, GTA weld in, tensile strength 284(T)
sheet, GTA weld in, yield strength 284(T)
sheet products 91
sheet, reduction in area 284(T)
sheet, tensile strength 284(T)
sheet, yield strength 284(T)
solution treating cycles (AMS 5667) 140(T)
solution treating cycles (AMS 5668) 140(T)
specific heat capacity 246(T)
straddle milling 191(T)
stress relieving 137(T)
stress-rupture strength 14(T) 19(F)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel X-750 (Cont.)
tapping 191(T)
tensile elongation 12(T)
tensile properties 283 284(T) 285(T)
thermal conductivity 247(T)
thermal treatments for precipitation hardening of
various forms 228 229(T)
threading 191(T)
turning 191(T)
ultimate tensile strength 12(T)
yield strength (0.2% offset) 12(T)
Inconel 751
composition 5(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
forgeability rating 93(T)
forging temperature 93(T)
Inconel 792 (IN -792)
aging cycles 141(T)
aircraft applications 261
applications, high-temperature 23
as columnar grain directionally solidified
alloy 267
columnar grain directionally solidified,
development 343
composition 6(T)
density 262(T)
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
gamma prime solvus temperature 325(T)
hot corrosion 308 309
hot corrosion resistance from alloying
elements 304
incipient melting temperature 325(T)
mean coefficient of thermal expansion 262(T)
melting range 262(T)
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 792 (IN -792) (Cont.)
SCDS, creep-rupture life, orientation effect 274 276(F)
SCDS, development 343
SCDS, high-angle boundaries effect on rupture
life 271(F)
solution treating cycles 141(T)
specific heat 262(T)
stress-rupture curve 259(F)
stress-rupture strength 18(T)
temperature-strength capability as function of
year of availability 350(F)
tensile elongation 16(T)
thermal conductivity 262(T)
turbine engine applications 267
ultimate tensile strength 16(T)
yield strength 239
yield strength (0.2% offset) 16(T)
Inconel 901 (IN -901)
aging cycles 140(T)
aircraft applications 91
density 246(T)
dynamic modulus of elasticity 245(T)
electrical resistivity 247(T)
elongation 233(T)
eta phase formation 363(F)
forgeability rating 102(T)
forging, design guides 95(T)
forgings, tensile properties of two test
coupons 232 233(T)
forging temperature 102(T)
gamma prime solvus temperature 324(T)
incipient melting temperature 324(T)
Laves phase formation 363(F)
mean coefficient of thermal expansion 247(T)
melting range 246(T)
nickel-base, eta phase role in strengthening 225
Index Terms Links
This page has been reformatted by Knovel to provide easier navigation.
Inconel 901 (IN -901) (Cont.)
reduction in area 233(T)
rupture strength vs. temperature 243(F)
solution treating cycles 140(T)
specific heat capacity 246(T)
stress-rupture strength 14(T)
tensile elongation 13(T)
thermal conductivity 247(T)
ultimate tensile strength 13(T) 233(T)
yield strength 233(T)
yield strength (0.2% offset) 13(T)
Inconel MA-754
aerospace applications 120(T)
aircraft applications 131 133
brazing 183
as common ODS alloy 129
composition 129(T) 132
creep-rupture strength 23
drilling hole sizes 199(T)
drilling speeds and feeds grouping 198(T)
electrical resistivity 250(T)
elongation 250(T)
gamma prime solvus temperature 325(T)
incipient melting temperature 325(T)
mean coefficient of thermal expansion at
538 C 250(T)
melting range 250(T)
nonradioactive dispersoid 132
1000h rupture strength MPa(ksi) 250(T)
as oxide-dispersion-strengthened alloy 28
plate production 131
product forms available 132(T)
production on a large scale 132
Top Related