SMAW Welding Techniques
![Page 2: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/2.jpg)
Weld Bead• A weld resulting from a pass
Stringer BeadWeave Bead
![Page 3: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/3.jpg)
Passes
• Weld Pass - A single progression of welding along a joint. The result of a pass is a weld bead or layer
![Page 4: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/4.jpg)
Root Pass Hot Pass
Fill Pass Cover Pass
![Page 5: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/5.jpg)
Techniques• Stringer (drag) (whip)• Weave
– Circles– crescent– zig zag– box weave– double J
![Page 6: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/6.jpg)
Progression (vertical)
• Up– deeper penetration – Higher deposit rate (lb/hr)– Use near 90 degree travel angle or slightly up
• Down – faster (point to point)– less penetration for thin metal– less dilution– Use steep grag angle
![Page 7: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/7.jpg)
Travel Speed
• Stay on the leading edge of the puddle
![Page 8: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/8.jpg)
Flat Position
• Fillet/Groove - stringer or weave, split bead or wide weave
![Page 9: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/9.jpg)
Horizontal• Fillet/Groove - stringers (small weave may be used in tight place)
• Bead Placement - bottom to top
![Page 10: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/10.jpg)
Vertical
• Fillet/Groove - weave (or whip but not straight stringers)
• Root pass 6010 whip
• Root pass 7018 straight stringer or weave (open closed)
![Page 11: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/11.jpg)
Overhead• Same as horizontal for Fillets
• 6010 open root whip for flat face and keyhole control
• 7018’s stringers
• OH Butt Joints can be stringers or weaves
![Page 12: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/12.jpg)
Dimensions
• Reinforcement -ASME flush 1/16 AWS flush 1/8 discuss keyholeing, metallic backing, nonmetallic backing, partial penetration, root openings, root faces, tacking, tack grinding, fast freeze, and fill freeze
• Fill -as many as needed 1/8 per pass flat overload 3/16 vertical
• Cover -flush 1/16 high, 1/16 past edge
![Page 13: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/13.jpg)
600 included angle
Root faces
Tacking
Feather Tacks
Butt Joint Preperation
1/16-1/8
(Joints without backing)
![Page 14: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/14.jpg)
Open Root Technique
• Use root opening to allow increase in amperage for smoother welding
• Whip backwards for penetration
• Whip forwards to reduce penetration
• Do Not Weave a root pass.
• Maintain a short arc gap
• Stay slightly in front of the puddle at all times. Use the keyholing technique.
![Page 15: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/15.jpg)
Root faces - 0
450 included angle
Remove all mill scales and rust
Tacking - not in groove
Tack away from coupon area.
Flush on backing
Butt Joint Preperation(With Backing)
![Page 16: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/16.jpg)
Welding grooves with Backing
• Keep the root opening wide
• Make the root pass in one bead
• Avoid tight areas at the weld toes
![Page 17: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/17.jpg)
Restarts
•Stagger all starts and stops or use run-on, run-off tabs
•Feather all restarts & start on top, or start in front and remelt
•Don’t restart in a coupon area.
•Also stagger all beads on a single pass.
•Use a longer arc length when starting a weld.Compare interpass grinding techniques vs. techniques for no interpass grinding.
![Page 18: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/18.jpg)
Craters
• Fill craters by reversing direction at the weld end
• Use a short arc length to control heat.
![Page 19: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/19.jpg)
Electrode Work Angles
450
300
700
![Page 20: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/20.jpg)
work angle (transverse angle)• middle of joint
• directs heat between sides
• may need to direct more on heavy plate
![Page 21: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/21.jpg)
Transverse Angle Effects
![Page 22: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/22.jpg)
Drag Angle increases Penetration
Increases crown height
Push Angle gives shallow penetration, and flattens out the weld surface.
Electrode Travel Angles
![Page 23: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/23.jpg)
Electrode (arc) Placement
Current takes the path of least resistance. Therefore, the arc, and resulting weld, will go where the electrode end is closest to, NOT NECESSARILY IN THE DIRECTION THE ELECTRODE IS POINTING
![Page 24: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/24.jpg)
Arc Length
•Longer arc lengths = increased puddle heat, flatter welds, deeper penetration
•Shorter arc lengths = less puddle heat, flatter welds, less penetration
•Use arc length to control puddle size, penetration, and burn through.
•Normal arc length is 1/16” - 1/8”
•Use a slightly longer arc length during a start or restart.
![Page 25: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/25.jpg)
Helpful Tips
•Clean your Welding Hood lens
•Drape the cable over your shoulder or knee
•Get Comfortable
•Watch the puddle, not the arc
•Concentrate on steady travel speed and arc length
![Page 26: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/26.jpg)
SMAW Machine Setup• DCEP (also called Direct Current Reverse Polarity)
• 77 - 150 Amp Range
• #5 fine amperage setting (approximately 110 amps)
• Connect work lead
• Set for Constant Current (Variable Voltage)
![Page 27: SMAW Powerpoint](https://reader033.fdocuments.net/reader033/viewer/2022061116/54669f8bb4af9f3f3f8b5368/html5/thumbnails/27.jpg)
Amperage Calculations
Range: 77 - 150
Fine tune dial: 0 - 10
Desired amperage: 105 amps
150 - 77 = 73
73 / 10 = 7.3
7.3 x 6 = 43.8
43.8 + 77 = 120.8
150 - 77 = 73
73 / 10 = 7.3
105 - 77 = 28
28 / 7.3 = 3.836
Range: 77 - 150
fine tune dial: 0 - 10