CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION
Transcript of CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION
![Page 1: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/1.jpg)
CHEMICALS FOR VAPOR AND
ATOMIC LAYER DEPOSITION
Harvard University October 4th, 2019
Strem Chemicals 1
NNCI ALD/MOCVD Symposium
![Page 2: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/2.jpg)
COMPANY HISTORY & BACKGROUND
1964 company founded,
manufacturing in Danvers, MA
1978 moved corporate HQ to
Newburyport, MA
1986 established European
HQ in Strasbourg, France
2014 Strem celebrated its
50th year anniversary
Global network of distributors
Europe, Asia, Middle East
5,000 Specialty Chemicals for
Research & Production
Custom Synthesis and cGMP
Manufacturing
World-wide customer base
2Strem Chemicals
Company Strategy: Provide specialty chemicals of high quality, in a timely fashion
![Page 3: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/3.jpg)
HUMAN RESOURCES
Small company with ~78 employees
many employees at company over 10 years, low
turnover
14 employees are Ph.D.’s
Approximately 1/4 each in manufacturing, customer
service, warehouse, administrative/facility
In 2006 Strem implemented an ESOP (Employee
Stock Ownership Program), making all employees
partial owners of Strem
3
Strem Chemicals
![Page 4: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/4.jpg)
ENVIRONMENTAL, HEALTH, SAFETY + SECURITY (EHS+S)
Strem is a member of SOCMA (Society of Chemical Manufacturer’s and Affiliates)
Safety is of primary importance
Strem subscribes to SOCMA’s EHS+S program
Regular training of staff, internal and external audits
First Responders trained from lab and warehouse
2012-2019 Gold, Silver and Bronze Performance Improvement Awards from SOCMA for outstanding commitment to continuous improvement in EHS&S practices.
ISO 9001:2015 certified
Strem Chemicals
4
![Page 5: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/5.jpg)
PRODUCT & MARKETS SERVED
5
Key Product Lines(product booklets available)
Metal Catalysts LigandsMOCVD/CVD
/ALD precursorsNanomaterials
Markets
Served
Pharmaceutical
Chemical/Petrochemical
Micro
ElectronicsVarious
markets
Academic / Government Research Centers
Customer base is globalStrem Chemicals
![Page 6: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/6.jpg)
HOW STREM BUILDS IN HIGH QUALITY:
Raw Materials
Reaction
Vessel
Environment
Product Isolation
Purification
Packaging
Handling
QC
Analytical
Strem Chemicals
High Quality is built into the product at each step
Picking
Shipping 6
material of composition,
cleaning, dedicated equipment
external- clean room
internal- dry, filtered gas
Metal sources 99.99 – 99.9999%
Organics 95 – 99%
Distillation, sublimation,
recrystallization
![Page 7: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/7.jpg)
MORE THAN 450 METAL PRECURSORS FOR CVD, ALD
Strem has a broad range of CVD/ALD precursors
7
Metal alkyls
Metal alkylamides and alkylimides
Metal Amidinates Volatile metal carbonyls
Metal alkoxides
Metal betadiketonates (and ligands)
Volatile organometallics, MetalCps
Metal Halides Strem Chemicals
![Page 8: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/8.jpg)
VOLATILE PRECURSORS FOR CVD, ALD ON STREM WEBSITE
8Strem Chemicals
![Page 9: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/9.jpg)
New products for ALD/CVD (2018-2019)
03-8000
79-1700 DIPAS, 14-1560
40-1028
64-6000
57-1500
78-1375
12-0865
22-1155
Strem Chemicals9
![Page 10: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/10.jpg)
o Volatile, air, light and thermally stable precursor
o 79-1700,(N,N-Diethyldithiocarbamato)dimethylgold(III), 97% (99.999%-Au) PURATREM
Thermal Atomic Layer Deposition of Continuous and Highly Conducting Gold Thin Films
University of Helsinki
1. Chem. Mater., 2017, 29 (14), 6130–6136
2. Journal of Crystal Growth 2015, 414, 143-150
3. Physics Procedia 2013, 46, 167-173
4. Gold Bulletin (Berlin, Germany) 2011, 44(3), 177-184
Gold ALD/CVD Precursor
Strem Chemicals
10
![Page 11: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/11.jpg)
NEW PRODUCTS IN DEVELOPMENT;
STREM # 44-5150 AND 78-0550.
11
44-5150
Focused electron beam-induced deposition precursor for
Ru and Pt;
Allylruthenium(II) tricarbonyl bromide
Lisa McElwee-White, University of Florida
Volatile material, sublimes at room temperature at 100 mTorr.
Cis-Dichlorodicarbonylplatinum(II).
Used for focused electron beam induced deposition of Pt
78-0550
![Page 12: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/12.jpg)
HIGH PRESSURE CAPABILITIES AT STREM CHEMICALS – METAL CARBONYLS
In 1964, Strem Chemicals, Inc. began manufacturing metal carbonyls
and metal carbonyl derivatives utilizing two, stainless steel, high pressure reactors
27-0400, Cobalt carbonyl (Dicobalt octacarbonyl)Strem Chemicals
12
![Page 13: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/13.jpg)
CCTBA IS USED FOR COBALT DEPOSITION
COBALT CARBONYL IS THE PRECURSOR
CCTBA
Strem 27-0770Dicobalt Octacarbonyl
Strem 27-0400
http://semimd.com/chipworks/2017/12/18/
iedm-2017-intels-10nm-platform-process/
Strem Chemicals
13
![Page 14: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/14.jpg)
Strem Chemicals 14
![Page 15: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/15.jpg)
Strem Chemicals 15
![Page 16: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/16.jpg)
Strem Chemicals 16
![Page 17: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/17.jpg)
Strem Chemicals 17
![Page 18: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/18.jpg)
Strem Chemicals 18
![Page 19: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/19.jpg)
Strem Chemicals 19
![Page 20: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/20.jpg)
Strem Chemicals 20
![Page 21: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/21.jpg)
Strem Chemicals 21
Metal Amidinates
![Page 22: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/22.jpg)
PATENTED METAL AMIDINATES
22
Newest
Products
03-8000
Strem Chemicals
![Page 23: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/23.jpg)
STREM # 03-8000
(N,N-Di-i-propylacetamidinato)lithium, min. 97% (99.99+%-Li) PURATREM
Onset 268C
Ends 305C
2.47% residue
184.6C
322.6C
DSCTGA
Strem Chemicals
23
![Page 24: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/24.jpg)
STREM# 27-0485
ALD precursor
Deposition of cobalt thin films on ALD WN as a
glue layer for copper interconnects in micro-and nanoelectronics
High thermal stability at deposition
temperature (350°C)
Low TGA residual mass: 9%
Highly air and moisture sensitiveInorg. Chem., 2003, 24, 7951-7958.
24Strem Chemicals
Bis(N,N'-di-i-propylacetamidinato)cobalt(II), min. 98% Co(iPr-MeAMD)2
Bis(N,N'-di-i-propylacetamidinato)cobalt(II), min. 98% (99.99%-Co) PURATREM (Co(iPr-MeAMD)2)
STREM# 27-0486
![Page 25: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/25.jpg)
Strem Chemicals
STREM# 27-0485
BAD UNIT
SUBLIMATION
RECRYSTALIZATION
25
![Page 26: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/26.jpg)
25-0230
High thermal stability
Superior step coverage of Mn4N films
in holes with aspect ratios 52:1.
Roy Gordon‘s Powerpoint
J. Electrochem. Soc., 2011, 158, D248-D253.
26Strem Chemicals
Bis(N,N’-diisopropylpentylamidinato)manganese(II)
![Page 27: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/27.jpg)
STREM# 29-7100
Extremely low TGA residual mass: 0.7% (Negligible decomposition
happened during melting and evaporation)
High thermal stability:
Very stable even at 190°C (Typical substrate temperature for ALD
of copper using these precursors.)
Inorg. Chem., 2005, 44, 1728-1735.
27Strem Chemicals
Bis(N,N'-di-sec-butylacetamidinato)dicopper(I), 99%
![Page 28: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/28.jpg)
STREM# 57-1200
Volatile ALD lanthanum compound. (60 mTorr at 100°C)
High reactivity to H2O, O2 and NH3
Line starts at origin => No delay in Nucleation
Roy Gordon‘s Group
28Strem Chemicals
TRIS(N,N'-DI-I-PROPYLFORMAMIDINATO)LANTHANUM(III), (99.999+%-LA) PURATREM LA-FMD
![Page 29: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/29.jpg)
Strem Chemicals
STREM# 57-1200
29
![Page 30: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/30.jpg)
30
Bubblers for
MOCVD, CVD
Strem Chemicals
CVD Bubblers (150 – 1000+ml)
ALD CYLINDERS (50ML)
ALD Cylinders
![Page 31: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/31.jpg)
CVD BUBBLERS
https://www.strem.com/uploads/resources/documents/electropolished_stainless_steel_bubblers
_.pdf
Strem Chemicals
31
![Page 32: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/32.jpg)
ALD CYLINDERS
We offer a variety of precursors prepackaged in 50mL
Swagelok® Cylinders.
Strem Chemicals
32
![Page 33: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/33.jpg)
Filling, refilling & cleaning services
“Request to Fill/Refill Bubbler or Cylinder” form
SERVICES OFFERED
Strem Chemicals
33
![Page 34: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/34.jpg)
97-7000
7ML BUBBLER FOR CVD
THIS 7ML, ELECTROPOLISHED, VERTICAL STAINLESS STEEL BUBBLER IS PERFECT FOR LOW
VOLUME APPLICATIONS AND IS COMPATIBLE WITH MOST COMMON TOOL TYPES.
OUR SMALL BUBBLER WILL MAXIMIZE GAS CONTACT TIME, REDUCE THE AMOUNT OF
MATERIAL NEEDED TO RUN TRIALS WHILE PROVIDING THE SAME FUNCTIONS OF A
REGULAR BUBBLER.
Strem Chemicals
34
![Page 35: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/35.jpg)
HOW TO LOOK FOR CVD/ALD PRECURSORS & BUBBLERS/CYLINDERS ON THE STREM WEBSITE
Strem Chemicals
35
![Page 36: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/36.jpg)
ALD APPLICATION ISSUES: 28-1301
Case study; Blockages reported in ALD Nickelocene cylinders resulting in restricted or lost flow/material delivery
Outlet valve blockageSolids at VCR connection between
cylinder and valve
Strem Chemicals
Bis(cyclopentadienyl)nickel, 99% (Nickelocene)
36
![Page 37: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/37.jpg)
Closer inspection shows decomposition evident
Solids at top of cylinder near valve
assembly (viewed via sliced end of cylinder).
Decomposed (brown) material
coating fill port of cylinder.
ALD APPLICATION ISSUES
Strem Chemicals
37
![Page 38: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/38.jpg)
NiCp2 is prone to decomposition when subjected to
higher temperatures over long timeframes.
Experimental investigations of thermodynamic properties of organometallic compounds.Thesis; R.A. Siddiqui, section 4.1.3. University of Duisburg-Essen, 2009
Over a short timeframe this decomposition is not detected
Over time (15 hrs at 77 C), the mass loss becomes constant leaving 18% residual mass from decomposition.
Strem Chemicals
38
![Page 39: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/39.jpg)
Conclusion and Recommendations
• When selecting a precursor for ALD/CVD use, consider carrying out a more
prolonged “thermal stress test” as well as the routine shorter term thermal
analysis.
• When using Nickelocene, if practical run at lower temperatures (ie. < 70 C) to
avoid too much decomposition.
• Similarly, during “non-run time” periods consider decreasing the heat applied
• Where possible consider using an alternative thermally more stable material
such as Strem 28-0045.
28-0045
Strem Chemicals
39
![Page 40: CHEMICALS FOR VAPOR AND ATOMIC LAYER DEPOSITION](https://reader031.fdocuments.net/reader031/viewer/2022012101/6169f43d11a7b741a34d35d8/html5/thumbnails/40.jpg)
40
Corporate HQ
Newburyport, MA, USA
(48,000 sq feet)
Laboratory Chemicals cGMP (kilo-lab) High Pressure
-Lab scale to 22 L / 50L glass reactors-ancillary equipment (rotovap, filtration)For larger scale Strem works with partners
1L, 2L & 5, 25
gallon autoclaves
Strem Chemicals
THANK YOU !